Sign In | Join Free | My himfr.com
Home > Steel Flange >

ASTM B462 UNS N08020, Nickel Alloy Superalloy Pipe Flange, Oil and Gas

    Buy cheap ASTM B462 UNS N08020, Nickel Alloy Superalloy Pipe Flange, Oil and Gas from wholesalers
     
    Buy cheap ASTM B462 UNS N08020, Nickel Alloy Superalloy Pipe Flange, Oil and Gas from wholesalers
    • Buy cheap ASTM B462 UNS N08020, Nickel Alloy Superalloy Pipe Flange, Oil and Gas from wholesalers
    • Buy cheap ASTM B462 UNS N08020, Nickel Alloy Superalloy Pipe Flange, Oil and Gas from wholesalers
    • Buy cheap ASTM B462 UNS N08020, Nickel Alloy Superalloy Pipe Flange, Oil and Gas from wholesalers

    ASTM B462 UNS N08020, Nickel Alloy Superalloy Pipe Flange, Oil and Gas

    Ask Lasest Price
    Brand Name : Yuhong
    Model Number : SB462 NO8020
    Certification : ASTM B462 UNS N08020 Nickel Alloy 20 Superalloy Flange
    Price : Negotiable
    Payment Terms : L/C, , T/T
    Delivery Time : 7 days
    • Product Details
    • Company Profile

    ASTM B462 UNS N08020, Nickel Alloy Superalloy Pipe Flange, Oil and Gas

    ASTM B462 / ASME SB462 UNS N08020 Nickel Alloy 20 Superalloy Pipe Flange PT Available


    We are one of the biggest projects pipeline products supplier in China, Our products contain steel pipe/tube,fittings, flanges. With development more than10 years, we have accumulated a great many clients all around the world and Yuhong products also won the great praise among the customers.


    Alloy 20 will resist corrosion especially in those environments that contain chemicals like nitric acid, phosphoric acid, chlorides and sulfuric acid. Alloy 20 also has good mechanical properties at both ambient as well as elevated temperatures. Alloy 20 is often termed as a superalloy. ASTM B462/ ASME SB462 Uns N08020 Blind Flange has excellent resistance to general corrosion, pitting, and crevice corrosion in chemicals containing chlorides as well as in acidic medium or conditions that contain acidic solutions like sulfuric, phosphoric, and nitric acids.


    Alloy 20 Forged and Plate Flange

    ASTM B462 Alloy 20 Slip-On Flange
    ASTM B462 Alloy 20 Threaded Flange
    ASTM B462 Alloy 20 Weld Neck Flange
    ASTM B462 Alloy 20 Socket Weld Flange
    ASTM B462 Alloy 20 Blind Flange
    ASTM B462 Alloy 20 Reducing Flange
    ASTM B462 Alloy 20 Lap Joint Flange
    ASTM B462 Alloy 20 Plate Flange
    ASTM B462 Alloy 20 Orifice Flange
    ASTM B462 Alloy 20 Forged Flange
    ASTM B462 Alloy 20 Ring Type Joint Flange
    ASTM B462 Alloy 20 Square Flange

    Alloy 20 Flanges Equivalent Grades

    STANDARDWERKSTOFF NR.UNSAFNOREN
    Alloy 202.4660N08020Z2NCUD31-20AZNiCr20CuMo

    Mechanical Properties

    AlloyTensile Strength, min.Yield Strength, min.Elongation, min.Reduction of Area, min.
    ASTM B462ksiMPaksiMPa%%
    UNS N08020805513524130.050.0

    *All values shall be measured at room temperature.
    *Alloy 20 flanges shall be supplied in stabilized-annealed condition.


    Chemical Composition

    ElementWt, %
    Carbon [C]≤0.07
    Manganese [Mn]≤2.00
    Phosphorus [P]≤0.045
    Sulfur [S]≤0.035
    Silicon [Si]≤1.00
    Nickel [Ni]32.00~38.00
    Chromium [Cr]19.00~21.00
    Molybdenum [Mo]2.00~3.00
    Copper [Cu]3.00~4.00
    Niobium+Tantalum [Nb+Ta]8xCarbon~1
    IronRemainder

    *The tabulated values are abstracted from ASTM B462 Gr. UNS N08020.


    ASME SB462 Alloy 20 Slip on Flange Vs DIN 2.4660 Weld Neck Flange
    The ASME SB462 Alloy 20 Slip on Flange is slipped into the pipe and then the connection is made with the help of double weld- one on the backside of the flange and one in the front. Generally, the slip on flanges are more affordable than the weld neck flanges, but it can become expensive with the number of welding and inspections. Also, the strength of the slip on flange under any internal pressure is around 2/3rd, and fatigue strength is around 1/3rd of that of the weld neck flange

    The DIN 2.4660 Weld Neck Flange is easily recognizable by the tapered hub which comes from the bolted connection to the pipe. The connection is made here with the help of but twelding, and that helps in preventing any type of turbulence at the joint. It also minimizes erosion and reduces restriction in the product flow. The alloy 20 weld neck flanges offer enhanced strength under different types of environments.


    Application

    • Marine enviroments
    • Desalination systems
    • Flue gas desulfurization equipment
    • Reaction vessels for pharmaceutical production
    • ASTM B462 UNS N08020, Nickel Alloy Superalloy Pipe Flange, Oil and Gas
    Quality ASTM B462 UNS N08020, Nickel Alloy Superalloy Pipe Flange, Oil and Gas for sale
    Inquiry Cart 0
    Send your message to this supplier
     
    *From:
    *To: Yuhong Group Co.,Ltd
    *Subject:
    *Message:
    Characters Remaining: (0/3000)